Grade 06Cr18Ni11Ti
Corresponding Standard Q/RP 007-2018
Stainless steel wire rods
Classification Austenitic Stainless Steel
06Cr18Ni11Ti Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu N More
Minimum Value - - - - - 17 9 - - Ti≥5C
Maximum Value 0.08 1 2 0.045 0.03 19 12 0.75 0.1
06Cr18Ni11Ti Mechanical Properties
delivery condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Offline solution annealing + pickling 1010℃ ~ 1100℃ Rapid Cooling ≤680 ≥40 ≥65
Hot-rolled + pickled - ≤730 ≥40 ≥65