Grade 00Cr17
Corresponding Standard Q/RP 007-2018
Stainless Steel Wire Rod
Classification Ferritic Stainless Steel
00Cr17 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value - - - - - 16 - - -
Maximum Value 0.03 1 1 0.04 0.03 18 0.6 0.25 0.6
00Cr17 Mechanical Properties
delivery condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Annealing + Pickling 750°C ~ 850°C slow cooling or approximately 800°C fast cooling 400~490 ≥30 ≥65

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!