Grade 12NiCr3-2
Corresponding Standard ISO 4954-1-2024
Steels for cold heading and cold extruding - Technical delivery conditions - Part1: Non-alloy and alloy steels
Classification Alloy Steel
12NiCr3-2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu
Minimum Value 0.09 - 0.3 - - 0.4 0.5 -
Maximum Value 0.15 0.3 0.6 0.025 0.025 0.7 0.8 0.25
12NiCr3-2 Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Hardness
HBW
5<d≤40 +AC ≤500 ≥62
5<d≤40 +FP 130~180
2≤d≤5 +AR+C+AC ≤500 ≥64
5<d≤40 ≤480 ≥64
2≤d≤5 +AR+C+AC+LC ≤540 ≥62
5<d≤40 ≤520 ≥62
5<d≤10 +AC+C ≤620 ≥59
10<d≤40 ≤610 ≥59
①+AR=as hot-rolled;+AR or +PE=as hot-rolled or peeled;+AR+C=as hot-rolled+cold drawn;+AR+C+AC=as hot-rolled+cold drawn+spheroidized;+AR+C+AC+LC=as hot-rolled+cold drawn+spheroidized+skin passed;+AC= spheroidized ;+AC or +AC+PE=spheroidized or spheroidized+peeled;+AC+C=spheroidized +cold drawn;+FP=treated to ferrite-pearlite structure and hardness range;+AC+C+AC=spheroidized +cold drawn + spheroidized;+AC+C+AC+LC=spheroidized +cold drawn + spheroidized + skin passed
Approximate Comparison Table
International Organization for Standardization European Standard
ISO EN Numerical Grade
12NiCr3-2 12NiCr3-2 1.5701
12NiCr3-2 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!