Grade 022Cr17Ni12Mo2N
China ISC S31653
Old Grade
Corresponding Standard GB /T 1220-2007
Stainless Steel Bars
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
022Cr17Ni12Mo2N Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 16 10 2 0.1
Maximum Value 0.03 1 2 0.045 0.03 18 13 3 0.16
022Cr17Ni12Mo2N Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
d≤180 Solid Solution Treatment ≥550 ≥245 ≥40 ≥50 HBW:≤217
HRB:≤95
HV:≤220
• This does not apply to flat bars, but if required by the buyer, it shall be determined through negotiation between the supplier and the buyer.
1 Approximate Comparison Table
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade SS BS EN/BS
022Cr17Ni12Mo2N
(00Cr17Ni13Mo2N)
S31653 316LN SUS 316LN STS 316LN 316LN S31653 X2CrNiMoN 17-12-2
X2CrNiMoN 17-11-2
X2CrNiMoN 17-13-3
(X2CrNiMoN 18-13)
1.4429 Z2CND 17-13Az
Z3CND 17-12Az
X2CrNiMoN 17-13-3
X2CrNiMoN 17-12-2
1.4429
1.4406
2375 316S63
316S61
2 Approximate Comparison Table Stainless steels for cold heading and cold extruding
China Japan United States International Organization for Standardization European Standard
GB ISC JIS ASTM/AISI UNS ISO Numerical Grade EN Numerical Grade
022Cr17Ni12Mo2N
(00Cr17Ni13Mo2N)
S31653 SUS316LN 316LN S31653 X2CrNiMoN17-12-3 4429-316-53-I X2CrNiMoN17-12-3 1.4429

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!