Grade 06Cr13
S11306
Corresponding Standard NB /T 47010-2017
Stainless and Heat-Resisting Steel Forgings for Pressure Equipment
Classification Ferritic Stainless Steel
Properties Corrosion Resistance
06Cr13 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 11.5 -
Maximum Value 0.06 1 1 0.035 0.02 13.5 0.6
06Cr13 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
t≤150 A(800~900缓冷) ≥410 ≥205 ≥20 110~163
• Heat treatment status code: A= annealing; S= Solid solution; Ag= Aging; T= tempering

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!