Grade 022Cr19Ni10
S30403
Corresponding Standard NB /T 47010-2017
Stainless and Heat-Resisting Steel Forgings for Pressure Equipment
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
022Cr19Ni10 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 18 8
Maximum Value 0.03 1 2 0.035 0.015 20 12
022Cr19Ni10 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
t≤150 S(1010~1150快冷) ≥480 ≥210 ≥35 128~187
150<t≤300 S(1010~1150快冷) ≥460 ≥210 ≥35 121~187
• Heat treatment status code: A= annealing; S= Solid solution; Ag= Aging; T= tempering

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!