Grade 20NiCrMoS6-4
European Standard Steel Grade 1.6571
Corresponding Standard EN 10084-2008
Case Hardening Steels - Technical Delivery Conditions
Classification Alloy Steel
20NiCrMoS6-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.16 - 0.5 - 0.02 0.6 1.4 0.25
Maximum Value 0.23 0.4 0.9 0.025 0.04 0.9 1.7 0.35
20NiCrMoS6-4 Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
Semifinished products, bars Processed to a Certain Shearability (+S) ≤255
All product shapes Soft Annealing (+A) ≤229
Bar, wire, flat steel, forging Processed to a Certain Hardness (+TH) 179~229
Bar, forging Processed to Ferrite-Perlite Structure (+FP) 154~207