Grade 4340
Corresponding Standard ASTM A519/A519M-2024
Standard Specification for Seamless Carbon and Alloy Steel Mechanical Tubing
Classification Alloy Steel
4340 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu * Mo
Minimum Value 0.38 0.15 0.6 - - 0.7 1.65 - 0.2
Maximum Value 0.43 0.35 0.8 0.04 0.04 0.9 2 0.35 0.3
1 Approximate Comparison Table Structural Alloy Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
34CrNi3Mo
34CrNiMo
ZG34CrNiMo
SNCM447 4340 36CrNiMo6 34CrNiMo6
GS-34CrNiMo6V
35NCD6 34CrNiMo6 1.6582 36KH2N2MFA
38KH2N2MA
40KHN2MA
2541 817M40
2 Approximate Comparison Table Cast Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
ZG34CrNiMo
34CrNi3Mo
34CrNiMo
SNCM447 4340 36CrNiMo6 GS-34CrNiMo6V
34CrNiMo6
35NCD6 34CrNiMo6 1.6582 36KH2N2MFA
38KH2N2MA
40KHN2MA
2541 817M40

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!