Grade X3CrTi17
European Standard Steel Grade 1.4510
Corresponding Standard EN 10028-7-2016
Flat Products Made of Steels for Pressure Purposes - Part 7: Stainless Steels
Classification Ferritic Stainless Steel
X3CrTi17 Chemical Element Composition Content (%)
Component C Si Mn P S Cr More
Minimum Value - - - - - 16 Ti: [4(C+N)+0.15]~0.8②
Maximum Value 0.05 1 1 0.04 0.015 18
X3CrTi17 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
C:T ≤ 4 +A 420~600 long.:≥230
tr.:≥240
T<3mm, A80①
long.+tr. :≥23
T≥3mm, A②
long.+tr. :≥23
long.+ tr.: ≥27
• C=cold rolled strip;H=hot rolled strip;P=hot rolled plate
• +A=Annealed;+AT=Solution annealed
• B=width;T=thick
1 Approximate Comparison Table Other Stainless Steels
China Japan United States International Organization for Standardization Germany France European Standard
ISC JIS ASTM ISO Numerical Grade DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade
S11863 SUS 430LX S43035 X3CrTi 17 4510-430-35-I X6CrTi 17
(X8CrTi 17)
1.4510 Z8CT 17 X3CrTi 17 1.4510
2 Approximate Comparison Table Ferritic Stainless Steel
China Japan International Organization for Standardization European Standard
ISC JIS ISO Numerical Grade Numerical Grade
S11863 SUS430LX X2CrNb17 4510-430-36-X 1.4510
3 Approximate Comparison Table Ferritic Stainless Steel
Japan United States France European Standard Russia
JIS ASTM UNS NF EN/NF EN Numerical Grade GOST
SUS430LX 439 S43035 Z4CT17 X3CrTi17 1.4510 08KH17T