Grade 1Cr18Ni9
Corresponding Standard GB 5310-1995
Seamless Steel Tubes and Pipes for High Pressure Boiler
Classification Austenitic Stainless Steel
1Cr18Ni9 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu
Minimum Value - - - - - 17 8 -
Maximum Value 0.15 1 2 0.035 0.03 19 10 0.2
• Steel produced by oxygen converter and secondary refining outside the furnace has a nitrogen content not exceeding 0.008%
1Cr18Ni9 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
solution treatment ≥520 ≥205 ≥35
Approximate Comparison Table Austenitic Stainless Steel
China United States
GB ASTM/AISI
1Cr18Ni9 302TH

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!