Grade 13Cr11Ni2W2MoV
China ISC S47310
Old Grade
Corresponding Standard GB /T 1221-2007
Heat-resistant Steel Bars
Classification Martensitic Stainless Steel
13Cr11Ni2W2MoV Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo W V
Minimum Value 0.1 - - - - 10.5 1.4 0.35 1.5 0.18
Maximum Value 0.16 0.6 0.6 0.035 0.03 12 1.8 0.5 2 0.3
13Cr11Ni2W2MoV Mechanical Properties
diameter
d
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
d≤75(1) Quenching + Tempering
≥885
Quenching + Tempering
≥735
Quenching + Tempering
≥15
Quenching + Tempering
269~321
Annealing
≤269
d≤75(2) Quenching + Tempering
≥1080
Quenching + Tempering
≥885
Quenching + Tempering
≥12
Quenching + Tempering
311~388
Annealing
≤269
Approximate Comparison Table Martensitic Heat-Resistant Steel
China Russia
GB ISC GOST
13Cr11Ni2W2MoV
(1Cr11Ni2W2MoV)
S47310 13Х11Н2В2МФ

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!