Grade 07Cr17Ni12Mo2
China ISC S31609
Corresponding Standard GB /T 713.7-2023
Steel Plate,Sheet and Strip for Pressure Equipments Part7:Stainless Steel and Heat Resisting Steel
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
Density 8 g/cm3
07Cr17Ni12Mo2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value 0.04 - - - - 16 10 2 -
Maximum Value 0.1 1 2 0.035 0.015 18 14 3 0.1
07Cr17Ni12Mo2 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Solutioon treatment ≥515 ≥220 ≥40 HBW: ≤217
HRB: ≤95
HV: ≤220
20°C:
Long: ≥100
tr: ≥60
-196°C:
tr: ≥60
Approximate Comparison Table Austenitic Stainless Steel
China United States European Standard
GB ISC ASTM/AISI UNS EN Numerical Grade
07Cr17Ni12Mo2
(1Cr17Ni12Mo2)
S31609 316H S31609 X3CrNiMo 17-13-3 1.4436

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!