Grade 022Cr17Ni12Mo2N
China ISC S31653
Corresponding Standard GB /T 713.7-2023
Steel Plate,Sheet and Strip for Pressure Equipments Part7:Stainless Steel and Heat Resisting Steel
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
Density 8.04 g/cm3
022Cr17Ni12Mo2N Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 16 10 2 0.1
Maximum Value 0.03 1 2 0.035 0.015 18 13 3 0.16
022Cr17Ni12Mo2N Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Specified Plastic Yield Strength
Rp0.2
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Solutioon treatment ≥515 Rp0.2: ≥205
Rp1.0: ≥320
≥40 HBW: ≤217
HRB: ≤95
HV: ≤220
20°C:
Long: ≥100
tr: ≥60
-196°C:
tr: ≥60
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade SS BS EN/BS
022Cr17Ni12Mo2N
(00Cr17Ni13Mo2N)
S31653 316LN SUS 316LN STS 316LN 316LN S31653 X2CrNiMoN 17-12-2
X2CrNiMoN 17-11-2
X2CrNiMoN 17-13-3
(X2CrNiMoN 18-13)
1.4429 Z2CND 17-13Az
Z3CND 17-12Az
X2CrNiMoN 17-13-3
X2CrNiMoN 17-12-2
1.4429
1.4406
2375 316S63
316S61
2 Approximate Comparison Table Stainless Steels for Cold Heading and Cold Extruding
China Japan United States International Organization for Standardization European Standard
GB ISC JIS ASTM/AISI UNS ISO Numerical Grade EN Numerical Grade
022Cr17Ni12Mo2N
(00Cr17Ni13Mo2N)
S31653 SUS316LN 316LN S31653 X2CrNiMoN17-12-3 4429-316-53-I X2CrNiMoN17-12-3 1.4429