Grade SUS 201
Corresponding Standard JIS G 4303-2005
Stainless Steel Bars
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
SUS 201 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - 5.5 - - 16 3.5 -
Maximum Value 0.15 1 7.5 0.06 0.03 18 5.5 0.25
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization European Standard
GB ISC CNS JIS KS ASTM UNS ISO EN Numerical Grade
12Cr17Mn6Ni5N
(1Cr17Mn6Ni5N)
S35350 201 SUS 201 STS 201 201 S20100 X12CrMnNi 17-7-5
X9CrMnNiCu17-8-5-2
X12CrMnNi 17-7-5
X9CrMnNiCu17-8-5-2
1.4372
1.4618
2 Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization European Standard
ISC JIS UNS ISO Numerical Grade Numerical Grade
S35350 SUS201 S20100 X12CrMnNiN17-7-5 4372-201-00-I 1.4372
3 Approximate Comparison Table Austenitic Stainless Steel
Japan United States France European Standard
JIS ASTM NF EN/NF EN Numerical Grade
SUS201 201 Z12CMN17-07Az X12CrMnNiN17-7-5 1.4372
SUS201 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!