Grade 07Cr19Ni10
Corresponding Standard GB 5310-2008
Seamless steel tubes and pipes for high pressure boiler
Classification Austenitic Stainless Steel
07Cr19Ni10 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu
Minimum Value 0.04 - - - - 18 8 -
Maximum Value 0.1 0.75 2 0.03 0.015 20 11 0.25
Approximate Comparison Table
China Japan United States International Organization for Standardization Germany European Standard
GB ISC JIS AISI UNS ISO DIN EN/DIN W-Nr. EN Numerical Grade
07Cr19Ni10 S30409 SUS 304H 304H S30409 X6CrNi 18-10
X7CrNi 18-9
X6CrNi18-10 1.4948 X6CrNi18-10 1.4948