Grade 10Cr18Ni12
China ISC S30510
Old Grade
Corresponding Standard GB /T 3280-2015
Cold rolled stainless steel plate and strip
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
10Cr18Ni12 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 17 10.5
Maximum Value 0.12 0.75 2 0.045 0.03 19 13
1 Approximate Comparison Table
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST BS EN/BS
10Cr18Ni12 S30510 305 SUS 305 STS 305 305 S30500 X6CrNi 18-12 X5CrNi 18-12
(X5CrNi 19-11)
X4CrNi 18-12
1.4303
1.4303
Z8CN 18-12 X4CrNi 18-12 1.4303 12Х18Н12Т 305S19
2 Approximate Comparison Table Stainless steels for cold heading and cold extruding
China Japan United States International Organization for Standardization European Standard
GB ISC JIS ASTM/AISI UNS ISO Numerical Grade EN Numerical Grade
10Cr18Ni12
(1Cr18Ni12)
S30510 SUS305 305 S30500 X6CrNi18-12 4303-305-00-I X6CrNi18-12 1.4303

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!