Grade 06Cr19Ni13Mo3
China ISC S31708
Old Grade
Corresponding Standard GB /T 4356-2016
Stainless Steel Wire Rod
Classification Austenitic Stainless Steel
06Cr19Ni13Mo3 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value - - - - - 18 11 3
Maximum Value 0.08 1 2 0.045 0.03 20 15 4
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States Germany United Kingdom
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. BS EN/BS
06Cr19Ni13Mo3 S31708 317 SUS 317 STS 317 317 S31700 X5CrNiMo 17-13 1.4449 317S16
2 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States Germany United Kingdom
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. BS EN/BS
06Cr19Ni13Mo3
(0Cr19Ni13Mo3)
S31708 317 SUS 317 STS 317 317 S31700 X5CrNiMo 17-13 1.4449 317S16
3 Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization European Standard
ISC JIS UNS ISO Numerical Grade Numerical Grade
S31708 SUS317 S31700 X6CrNiMo19-13-4 4445-317-00-U (1.4445)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!