Grade 10Cr17Mo
China ISC S11790
Corresponding Standard GB /T 4240-2019
Stainless steel wires
Classification Ferritic Stainless Steel
10Cr17Mo Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value - - - - - 16 - 0.75
Maximum Value 0.12 1 1 0.04 0.03 18 0.6 1.25
10Cr17Mo Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
1≤d≤3 Soft 480~650 ≥15
3<d≤16 Soft 450~650 ≥15
0.3≤d≤3 Light Drawing 530~780
3<d≤6 Light Drawing 500~750
6<d≤16 Light Drawing 480~730
①soft - Wire is subjected to bright heat treatment, or after heat treatment, it undergoes pickling or similar processes to remove surface scale.
②Lightly drawn- Wire is drawn to finished dimensions with a small reduction in cross-section after heat treatment.
③Cold drawn - Wire undergoes conventional drawing after heat treatment, which is the process of forming at room temperature through methods such as die drawing or roll drawing.
1 Approximate Comparison Table Ferritic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Sweden United Kingdom
GB ISC CNS JIS KS ASTM/AISI UNS ISO Numerical Grade DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade SS BS EN/BS
10Cr17Mo
(1Cr17Mo)
S11790 434 SUS 434 STS 434 434 S43400 X6CrMo 17-1
9c
(ISO 683-13-1986)
4113-434-00-I X6CrMo 17-1
(X6CrMo 17)
1.4113
1.4113
Z8CD 17-01 X6CrMo 17-1 1.4113 2325 434S17
434S19
2 Approximate Comparison Table Stainless Steels for Cold Heading and Cold Extruding
China Japan United States International Organization for Standardization European Standard
GB ISC JIS ASTM/AISI UNS ISO Numerical Grade EN Numerical Grade
10Cr17Mo
(1Cr17Mo)
S11790 SUS434 434 S43400 X6CrMo17-1 4113-434-00-I X6CrMo17-1 1.4113

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!