Grade 07Cr19Ni10
China ISC S30409
Corresponding Standard GB /T 4240-2019
Stainless steel wires
Classification Austenitic Stainless Steel
07Cr19Ni10 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value 0.04 - - - - 18 8
Maximum Value 0.1 1 2 0.045 0.03 20 11
1 Approximate Comparison Table
China Japan United States International Organization for Standardization Germany European Standard
GB ISC JIS AISI UNS ISO DIN EN/DIN W-Nr. EN Numerical Grade
07Cr19Ni10 S30409 SUS 304H 304H S30409 X6CrNi 18-10
X7CrNi 18-9
X6CrNi18-10 1.4948 X6CrNi18-10 1.4948
2 Approximate Comparison Table Seamless steel tubes and pipes for high pressure boiler
China United States European Standard
GB ISC ASTM/AISI EN
10Cr9MoW2VNbBN S30409 SA-213 TP304H X6CrNi18-10

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!