Grade X12NiCrSi 35-16
European Standard Steel Grade 1.4864
Corresponding Standard EN 10088-1-2005
Staehle Stainless steels. Part 1:List of stainless steels
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
Density 8 g/cm3
X12NiCrSi 35-16 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - 1 - - - 15 33 -
Maximum Value 0.15 2 2 0.045 0.015 17 37 0.11
① Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. All appropriate precautions are to be taken to avoid the addition of such elements from scrap and other materials used in production which would impair mechanical properties and the suitability of the steel.
1 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade BS EN/BS
12Cr16Ni35
(1Cr16Ni35)
S33010 SUH 330 SUH 330 STR 330 330 N08330 X12CrNiSi 35-16 X12NiCrSi 36-16 1.4864 Z12NCS 35-16
Z12NC 37-18
X12NiCrSi 35-16 1.4864 NA 17
2 Approximate Comparison Table Austenitic Stainless Steel
China Japan International Organization for Standardization European Standard
ISC JIS ISO Numerical Grade Numerical Grade
S33010 SUH330 X13NiCr35-16 4864-083-77-X 1.4864
3 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Japan United States International Organization for Standardization Germany France European Standard
GB JIS ASTM ISO DIN EN/DIN NF EN/NF EN Numerical Grade
1Cr16Ni35 SUH330 330 H17 X12NiCrSi36-16 Z12NCS37-18 X12NiCrSi35-16 1.4864

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!