Grade X17CrNi 16-2
European Standard Steel Grade 1.4057
Corresponding Standard EN 10250-4-1999
Classification Martensitic Stainless Steel
Properties Corrosion Resistance
X17CrNi 16-2 Chemical Element Composition Content (%)
Component C Si Mn P S * Cr Ni
Minimum Value 0.12 - - - - 15 1.5
Maximum Value 0.22 1 1.5 0.04 0.03 17 2.5
X17CrNi 16-2 Mechanical Properties
thickness
t
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
t≤250 A ≤1000 - - ≤295 -
t≤250* QT800 800~950 ≥600 ≥10 - ≥20
t≤250** QT800 800~950 ≥600 ≥8 - ≥15
t≤250* QT900 900~1050 ≥700 ≥10 - ≥15
t≤250** QT900 900~1050 ≥700 ≥8 - ≥10
1 Approximate Comparison Table Martensitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO Numerical Grade DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
14Cr17Ni2
(1Cr17Ni2)
17Cr16Ni2
S43110
/
S43120
431 SUS 431 STS 431 431 S43100 X17CrNi 16-2 4057-431-00-X X20CrNi 17-2
(X22CrNi 17)
1.4057 Z15CN 16-02 X17CrNi 16-2 1.4057 14Х17Н2 2321 431S29
2 Approximate Comparison Table Martensitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
14Cr17Ni2
(1Cr17Ni2)
S43110 431 SUS 431 STS 431 431 S43100 X20CrNi 17-2
(X 22CrNi 17)
1.4057 Z15CN 16-02 X17CrNi 16-2 1.4057 14Х17Н2 2321 431S29
3 Approximate Comparison Table Martensitic Heat-Resistant Steel
China United States Germany European Standard Russia
GB ASTM DIN EN/DIN EN Numerical Grade GOST
1Cr17Ni2
ML1Cr17Ni2
431 X17CrNi16-2 X17CrNi16-2 1.4057 14KH17N2
20KH17N2