Grade X17CrNi 16-2
European Standard Steel Grade 1.4057
Corresponding Standard EN 10088-1-2005
Staehle Stainless steels. Part 1:List of stainless steels
Classification Martensitic Stainless Steel
Properties Corrosion Resistance
Density 7.7 g/cm3
X17CrNi 16-2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value 0.12 - - - - 15 1.5
Maximum Value 0.22 1 1.5 0.04 0.015 17 2.5
① Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. All appropriate precautions are to be taken to avoid the addition of such elements from scrap and other materials used in production which would impair mechanical properties and the suitability of the steel.
1 Approximate Comparison Table Martensitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO Numerical Grade DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
14Cr17Ni2
(1Cr17Ni2)
17Cr16Ni2
S43110
/
S43120
431 SUS 431 STS 431 431 S43100 X17CrNi 16-2 4057-431-00-X X20CrNi 17-2
(X22CrNi 17)
1.4057 Z15CN 16-02 X17CrNi 16-2 1.4057 14Х17Н2 2321 431S29
2 Approximate Comparison Table Martensitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
14Cr17Ni2
(1Cr17Ni2)
S43110 431 SUS 431 STS 431 431 S43100 X20CrNi 17-2
(X 22CrNi 17)
1.4057 Z15CN 16-02 X17CrNi 16-2 1.4057 14Х17Н2 2321 431S29
3 Approximate Comparison Table Martensitic Heat-Resistant Steel
China United States Germany European Standard Russia
GB ASTM DIN EN/DIN EN Numerical Grade GOST
1Cr17Ni2
ML1Cr17Ni2
431 X17CrNi16-2 X17CrNi16-2 1.4057 14KH17N2
20KH17N2