Grade 07Cr17Ni7Al
China ISC S51770
Old Grade
Corresponding Standard GB /T 4239-1991
Cold rolled stainless steel and heatresisting steel strip
Classification Precipitation-Hardening Stainless Steel
Properties Corrosion Resistance
Density 7.81 g/cm3
07Cr17Ni7Al Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Al
Minimum Value - - - - - 16 6.5 0.75
Maximum Value 0.09 1 1 0.035 0.03 18 7.75 1
07Cr17Ni7Al Mechanical Properties
thickness
t
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
/(solution) ≤1030 ≤380 ≥20 HV
≤200
≤3 (565°C aging) ≥1140 ≥960 ≥3 HV
≥345
>3 ≥1140 ≥960 ≥5 ≥345
≤3 (510°C aging) ≥1225 ≥1030 HV
≥392
>3 ≥1225 ≥1030 ≥4 ≥392
1 Approximate Comparison Table
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST
07Cr17Ni7Al
(0Cr17Ni7Al)
S51770 631 SUS 631 STS 631 631 S17700 X7CrNiAl 17-7
2
(ISO 683-13-1986)
X7CrNiAl 17-7 1.4568 Z8CNA 17-07 X7CrNiAl 17-7 1.4568 09Х17Н7Ю
2 Approximate Comparison Table
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST
07Cr17Ni7Al
(0Cr17Ni7Al)
S51770 631 SUS 631 STS 631 631 S17700 X7CrNiAl 17-7 X7CrNiAl 17-7 1.4568 Z8CNA 17-07 X7CrNiAl 17-7 1.4568 09Х17Н7Ю

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!