Grade 022Cr17Ni7N
China ISC S30153
Corresponding Standard GB /T 20878-2007
Stainless and Heat-Resisting Steels - Designation and Chemical Composition
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
Density 7.93 g/cm3
022Cr17Ni7N Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - - - - 16 5 0.07
Maximum Value 0.03 1 2 0.045 0.03 18 8 0.2
Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization European Standard
ISC JIS ASTM UNS ISO Numerical Grade EN Numerical Grade
S30153 SUS 301L 301LN S30153 X2CrNiN18-7 4318-301-53-I X2CrNiN18-7 1.4318
022Cr17Ni7N Corresponding Standards(Same grade name, different standards)