Grade 16Cr23Ni13
China ISC S30920
Old Grade
Corresponding Standard GB /T 1221-2007
Heat-resistant Steel Bars
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
16Cr23Ni13 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 22 12
Maximum Value 0.2 1 2 0.04 0.03 24 15
16Cr23Ni13 Mechanical Properties
diameter
d
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
d≤180 (solution treatment) ≥560 ≥205 ≥45 ≤201
Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States Germany France European Standard Russia United Kingdom
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST BS EN/BS
16Cr23Ni13
(2Cr23Ni13)
S30920 SUH 309 SUH 309 STR 309 309 S30900 X15CrNiSi 20-12 1.4828 Z15CNS 20-12 X15CrNiSi 20-12 1.4828 20Х20Н14С2 309S24

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!