Grade 06Cr23Ni13
China ISC S30908
Old Grade
Corresponding Standard GB /T 1221-2007
Heat-Resistant Steel Bars
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
06Cr23Ni13 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 22 12
Maximum Value 0.08 1 2 0.045 0.03 24 15
06Cr23Ni13 Mechanical Properties
diameter
d
mm
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
d≤180 (solution treatment) ≥520 ≥205 ≥40 ≤187
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST
06Cr23Ni13
(0Cr23Ni13)
S30908 309S SUS 309S STS 309S 309S S30908 X12CrNi 23-13
X6CrNi23-13
X7CrNi 23-14 1.4833 Z15CN 24-13 X12CrNi 23-13
X6CrNi23-13
1.4833
1.4950
10Х23Н13
2 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST
06Cr23Ni13
(0Cr23Ni13)
S30908 309S SUS 309S STS 309S 309S S30908 X12CrNi 23-13 X7CrNi 23-14
X12CrNi 23-13
1.4833
1.4833
Z15CN 24-13 X12CrNi 23-13 1.4833 10Х23Н13
3 Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization European Standard
ISC JIS UNS ISO Numerical Grade Numerical Grade
S30908 SUH309 S30908 X18CrNi23-13 4833-309-08-I 1.4833

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!