Grade 4130
Corresponding Standard ASTM A866-2014
Medium Carbon Anti-Friction Bearing Steel
Classification Bearing Steel
4130 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu Mo Al O
Minimum Value 0.28 0.15 0.4 - - 0.8 - 0.15 - -
Maximum Value 0.33 0.35 0.6 0.025 0.025 1.1 0.3 0.25 0.05 0.002
Note1: Elements not quoted shall not be intentionally added to the steel without the agreement of the purchaser
Note2: Intentional additions of calcium or calcium alloys for deoxidation or inclusion shape control are not permitted unless specifically approved by the purchaser
Note3: Oxygen content applies to product analysis and shall be determined in accordance with Test Methods E1019.
1 Approximate Comparison Table Structural Alloy Steel
China Japan United States Germany France European Standard Russia Sweden
YB ISC JIS ASTM DIN EN/DIN W-Nr. L-Nr. NF EN/NF EN Numerical Grade GOST SS14
25CrMo A30252 SCM430 4130 25CrMo4 1.7218 1.7214 25CD4 25CrMo4 1.7218 30ХМ 2225
2 Approximate Comparison Table Structural Alloy Steel
China Taiwan, China Japan South Korea United States France European Standard
GB ISC CNS JIS KS ASTM NF EN/NF EN
30CrMo A30302 SCM430 SCM430 SCM430 4130 30CD4 34CrMo4
3 Approximate Comparison Table Structural Alloy Steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS SAE ISO DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
30CrMo SCM420
SCM430
4130 25CrMo4 25CrMo4 25CD4 25CrMo4 1.7218 20KHM
30KHM
30KHMA
2225 708A25
708M25
CFS10